General Sales Conditions
 


Non Toxic Anticorrosive Pigments in Powder

Attributes

Habicor CP 4295

(Chrome Phosphate)

Habicor ZP 3850

(Zinc Phosphate)

Cr calc. as CrO3
24 - 27 %
/
Zn calc. as ZnO
/
50.5 - 52.0 % 1)
P calc. as P2O5
44 - 48 %
47 - 50 % 1)
Cl-
max. 0.05 %
max. 0.05 %
SO42-
max. 0.1 %
max. 0.1 %
loss on ignition (600 ° C)
26 - 29 %
8 - 16 %
moisture
max. 7 %
max. 0.2 %
conductivity
max. 500 µS cm-1
120 µS cm-1
pH value
5.5 - 6.5
6.0 - 8.0
oil absorption
65 ± 10 %
20 ± 10 %
residue on sieve (45 µm mesh)
max. 0.2 %
max. 0.2 %
median particle size
max. 2 µm
max. 8 µm
mean fraction
max. 3 µm
max. 8 µm
fineness
max. 50 µm
max. 35 um
fastness to heat

120 ° C

180 ° C
tamped density 0.8 kg/l 0.9 kg/l

Attributes

Habicor ZN

(co-precipitated, phosphate based)

Habicor ZC

(co-precipitated, phosphate based)

Zn calc. as ZnO
63.6 % 1)
46.8 % 1)
P calc. as P2O5
26 - 27 % 1)
47 - 49 % 1)
Ca calc. as CaO
/
12 - 16 %
Cl-
max. 0.05 %
max. 0.05 %
SO42-
max. 0.1 %
max. 0.1 %
loss on ignition (600 ° C)
max. 10 %
max. 10 %
moisture
max. 1 %
max. 1 %
conductivity
max. 250 µS cm-1
max. 250 µS cm-1
pH value
6.5 - 7.5
7.0 - 8.5
oil absorption 25 ± 10 % 25 ± 10 %
residue on sieve (45 µm mesh)
0.03 %
0.02 %
median particle size
max. 6 µm
max. 4 µm
mean fraction
max. 7 µm
max. 5 µm
fineness
max. 50 µm
max. 20 µm
BET
n.a.
8.9 m2/g
fastness to heat

160 ° C

160 ° C
tamped density 0.6 kg/l 0.6 kg/l

Attributes

Habicor ZM

(co-precipitated, phosphate based)

Habicor ZO

(co-precipitated, phosphate based)

Zn calc. as ZnO
50.3 % 1)
50.5 % 1)
P calc. as P2O5
34 - 36 % 1)
28 - 30 % 1)
Mo calc. as MoO3
1.0 %
/
Cl-
max. 0.05 %
max. 0.05 %
SO42-
max. 0.1 %
max. 0.1 %
loss on ignition (600 ° C)
max. 10 %
max. 10 %
moisture
max. 1 %
max. 1 %
conductivity
max. 250 µS cm-1
max. 250 µS cm-1
pH value
7.0 - 8.5
7.0 - 8.5
oil absorption
25 ± 10 %

25 ± 10 %

residue on sieve (45 µm mesh)
0.02 %
0.02 %
median particle size
max. 5 µm
max. 4 µm
mean fraction
max. 6 µm
max. 20 µm
fineness
max. 20 µm
max. 20 µm
BET
11.4 m2/g
11.8 m2/g
fastness to heat

160 ° C

160 ° C
tamped density 0.6 kg/l 0.6 kg/l
 

    1) according to ISO 6745:1990

back